Vacuum forming mold design guide

Shrinkage and Mold Sizing

Formed plastic shrinks as it cools, so the mold has to be slightly larger than the part you want. How much depends on the material.

Why it matters

If parts must fit a product, a lid or another part, shrinkage decides whether they do. A mold cut to exact part size will make parts that are too small. The mold is scaled up by the material's shrink factor so the cooled part lands on size.

Sheet materialTypical shrink (approx.)
PET / PETGabout 0.3% to 0.6%
PVCabout 0.3% to 0.6%
HIPS (polystyrene)about 0.3% to 0.6%
ABSabout 0.4% to 0.8%
Acrylicabout 0.4% to 0.8%
Polycarbonateabout 0.5% to 0.8%
Polypropyleneabout 1% to 2%
HDPEabout 2% to 3%

Check with your sheet supplier

These ranges are approximate. Shrink varies with sheet grade, thickness, mold temperature and cycle time, so confirm values with your sheet supplier and, for tight-tolerance parts, form a prototype and measure before cutting the production mold.

Male vs. female

Remember which surface is controlled. A female mold controls the outside of the part; a male mold controls the inside. Design the mold to the surface that has to fit.

Written by Shaun Butler, a mechanical design engineer who has machined thermoforming molds, master tooling and plug assists for packaging and medical customers for many years, and a former lead engineer and VP of Operations at Count Machinery.

Need a mold made?

Prototype molds in days, aluminum production molds in about 1–2 weeks.

Request a quote